Grade | Ni% | Mn% | Fe% | Si% | Cr% | C% | Cu% | S% |
Alloy 600 | Min 72.0 | Max 1.0 | 6.0-10.0 | Max 0.50 | 14-17 | Max 0.15 | Max 0.50 | Max 0.015 |
Grade | Density | Melting Point |
Alloy 600 | 8.47 g/cm3 | 1370°C-1413 °C |
Grade | British Standard | Werkstoff Nr. | UNS |
Alloy 600 | BS 3075 (NA14) | 2.4816 | N06600 |
Alloy State | Tensile Strength | Yield Strength | Elongation | Brinell Hardness (HB) |
Annealing Treatment | 550 N/mm² | 240 N/mm² | 30% | ≤195 |
Solution Treatment | 500 N/mm² | 180 N/mm² | 35% | ≤185 |