- Cold rolled strips: 0.03~0.l0×180~250mm >0.10~1.00×10~250mm >1.00~2.50×100~250mm 2. Cold drown wires: 0.l0~6.00mm 3. Hot rolled flat products: 4.50~20.0×50~250mm 4. Hot forged bars: Φ20.0~100.0mm / bar
Grade | Chemical composition(%) | |||||||||
C | P | S | Mn | Si | Ni | Cr | Mo | Cu | Fe | |
Max | ||||||||||
1J50 | 0.03 | 0.020 | 0.020 | 0.30~0.60 | 0.15~0.30 | 49.0~51.0 |
|
| ≤0.20 | Rest |
Density (g/cm3) | 8.2 |
Electrical resistivity at 20℃(Ωmm2/m) | 0.45 |
Coefficient of linear expansion(20℃~200℃)X10-6/℃ | 9,2 |
Saturation magnetostriction coefficient λθ/ 10-6 | 25,0 |
Curie point Tc/ ℃ | 500 |
The magnetic properties of alloys with high permeability in weak fields | ||||
1J50 | Initial permeability | Maximum permeability | Coercivity | Saturation magnetic induction intensity |
Сold-rolled strip/ sheet. Thickness, mm | μ0.08/ (mH/m) | μm/ (mH/m) | Hc/ (A/m) | BS/ T |
≥ | ≤ | |||
0.05 mm | 2.5 | 35 | 20 | 1.5 |
0.1~0.19 mm | 3.8 | 43.8 | 12 | |
0.2~0.34 mm | 4.4 | 56.3 | 10.4 | |
0.35~1.0 mm | 5.0 | 65 | 8.8 | |
1.1~2.5 mm | 3.8 | 44.0 | 12 | |
Bar | ||||
8-100 mm | 3.1 | 25.0 | 24 |